Surface inspection

Thin-film defect inspection

Compare photographs of six types of film defect with the corresponding CRD segmentation heatmaps.

Localising defects on thin film

Both views show the same area of film. Pale yellow indicates a stronger model response and dark purple a weaker one.

Localising defects on thin film · Inspection image
Inspection image
Localising defects on thin film · CRD segmentation heatmap
CRD segmentation heatmap
Model response01

Explore by defect type

These 18 image pairs come from the held-out defect set. Select a defect type to compare each photograph with its model output.

Aged adhesive

Sample 0363

Detected
Aged adhesive · Sample 0363 · Inspection image
Inspection image
Aged adhesive · Sample 0363 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0806

Detected
Aged adhesive · Sample 0806 · Inspection image
Inspection image
Aged adhesive · Sample 0806 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0828

Detected
Aged adhesive · Sample 0828 · Inspection image
Inspection image
Aged adhesive · Sample 0828 · CRD segmentation heatmap
CRD segmentation heatmap

Thin spots

Sample 1174

Detected
Thin spots · Sample 1174 · Inspection image
Inspection image
Thin spots · Sample 1174 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0169

Detected
Thin spots · Sample 0169 · Inspection image
Inspection image
Thin spots · Sample 0169 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 1182

Detected
Thin spots · Sample 1182 · Inspection image
Inspection image
Thin spots · Sample 1182 · CRD segmentation heatmap
CRD segmentation heatmap

Holes

Sample 0768

Detected
Holes · Sample 0768 · Inspection image
Inspection image
Holes · Sample 0768 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0770

Detected
Holes · Sample 0770 · Inspection image
Inspection image
Holes · Sample 0770 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0769

Detected
Holes · Sample 0769 · Inspection image
Inspection image
Holes · Sample 0769 · CRD segmentation heatmap
CRD segmentation heatmap

Insects

Sample 1136

Detected
Insects · Sample 1136 · Inspection image
Inspection image
Insects · Sample 1136 · CRD segmentation heatmap
CRD segmentation heatmap

Surface contamination

Sample 0466

Detected
Surface contamination · Sample 0466 · Inspection image
Inspection image
Surface contamination · Sample 0466 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0661

Detected
Surface contamination · Sample 0661 · Inspection image
Inspection image
Surface contamination · Sample 0661 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0079

Detected
Surface contamination · Sample 0079 · Inspection image
Inspection image
Surface contamination · Sample 0079 · CRD segmentation heatmap
CRD segmentation heatmap

Edge defects

Sample 1195

Detected
Edge defects · Sample 1195 · Inspection image
Inspection image
Edge defects · Sample 1195 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 1263

Detected
Edge defects · Sample 1263 · Inspection image
Inspection image
Edge defects · Sample 1263 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0202

Detected
Edge defects · Sample 0202 · Inspection image
Inspection image
Edge defects · Sample 0202 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 0945

Detected
Edge defects · Sample 0945 · Inspection image
Inspection image
Edge defects · Sample 0945 · CRD segmentation heatmap
CRD segmentation heatmap

Sample 1250

Missed
Edge defects · Sample 1250 · Inspection image
Inspection image
Edge defects · Sample 1250 · CRD segmentation heatmap
CRD segmentation heatmap

Held-out evaluation

Held-out defect photographs
1,341
Detection rate on defect photographs
97.54%

The test images were held apart from training and validation. At the selected alarm threshold, 97.54% of the defect photographs triggered an alert. Assessing the production false-alarm rate still requires photographs of defect-free film.